High Temperature Water Based Paint

---

We are looking for an aqueous-based high temperature white and black material for spray.

Operating temp. of approx. 500° F.

Any such animal out there?

Jim Cummings
powder coating - Buffalo, New York


---

Sermatech makes a silver colored water based aluminum paint that has to be baked. Costs like $105 a gal and is not easy to put on in low or high humidity. Do not know if they have black. They have several applicator sites also. There are high temperature stoving enamels, but they are solvent based and must be baked also. Most colors are available in this, but some are not heat resistant.

James Watts
- Navarre, Florida

---

Dear Mr. Cummings:

Magni Industries has several water based coatings that can handle temperatures in excess of 500F. These coatings can be baked or air dried. Black and Grey are standard colors.

Edward Koneczny
- Birmingham, Michigan


April 12, 2011

We offer a water base paint (white) for hot steel mill products. This paint is applied over hot products within a 800-1600° F range.

al

ALBERTO MERCHIORI
ABM Marking - BELLEVILLE ILLINOIS

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search