We want to anodize MMC material (Al30Si70). Who has experience and can tell use about the procedure.

Any advice would be appreciated.

Jan-Henk Pennings
TNO METALS RESEARCH INSTITUTE


--

The Canning Handbook states that high Si alloys are unsuitable for anodizing. Perhaps someone is doing some research in this area, or you could tell us something you may have discovered. METALAST has set up a research laboratory for anodizing, and Anodizer's Plaza (available from our WWW links page) is also run by specialists at university.

Tom Pullizzi
Falls Township, Pennsylvania 

--

Please contact me to get more info. regarding the anodization of MMC which we successfully performed.

Samir Elomari
Canadan Space Agency


--

Proper netiquette demands, in public forums such as this, that information be freely shared on line, not in private correspondence. Each letter which is posted "improves the breed", as winners spawn other winners when playing the ponies. Letters sent in private do not share this benefit, as inbreeding causes the swift end of the question. It's the diminishing gene pool problem, no matter how smart the original pair of question/answer, you need to mix in some fresh ideas.


Tom Pullizzi
Falls Township, Pennsylvania

--

Thanks to Tom Pullizzi for the reference to METALAST. And yes, we do have a research and technology center dedicated to anodizing. While our technology is offered through our network of METALAST licensees, we are happy to work with anodizers interested in the METALAST technology and with manufacturers using anodizing in their manufacturing process. Te contact us and to learn more, please feel free to visit our website.

Thanks - and as always, our appreciation to finishing.com for the excellent forum they provide for metal finishing issues.

Len Semas, Chief Operating Officer
METALAST International, Inc.

Minden, Nevada


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search