Search for black plating for steel
bolt
Letter 10070
I have a steel bolt that I need to make black. It is being used on
a license plate. I have had some Black Zinc - ed and need to get some
information on rust, hardness etc. Is there a better finish/ plating
that I can use on a standard grade 2 bolt that will be harder
(resistant to scratches), blacker etc. I own a small company and
don't have a lot of expertise in this field. I currently nickel and
chrome plate these bolts. I need a black one.
Can someone help me?
Phoenix Fallon
- Goleta, California
See if one of your plating shops offers black chrome plating.
|
|

Ted Mooney, P.E.
finishing.com
Brick, New Jersey
|
I'd still recommend Zinc-iron with Silver free black instead of
black chrome.
|
Khozema
Vahanwala
Saify Ind
Bangalore, Karnataka, India
|
|
-
-
 |