Aluminum Blue 2LW Dye

I am in the process of testing per ASTM B136-84 [link is to spec at TechStreet] (Dye Stain Test) which requires the use of aluminum blue 2LW dye. The ASTM spec offers a footnote referencing a supplier as a source for this chemical that is no longer in business.

Does any one have a current source for chemical?

Stephen Keller
- Hunt Valley, Maryland


 

With all of the consolidations in the metal finishing businesses, it is very hard to keep up with. That dye is manufactured by Clarient Corp in Charlotte, NC. This dye likes to mold as bad as coffee does, so do not make up any more than you can use in a week or so, or keep it in the refrigerator.

James Watts
- Navarre, Florida

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search