Aluminum chemical cleaning
Letter 10061
I need to strip out a layer of a complexed material based on
Tungsten and Silicon from Aluminum surface. Looking for chemical
solutions with potential etching of the deposition and inert to the
Aluminum totally.
Thanks,
Gideon Drimer
- Jerusalem, Israel
As stated, it does not exist.
James Watts