HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 10052
Cleaning Brushed aluminum stove top
Dear Sirs:
I have a brushed aluminum stove top (not stainless steel) and I can't get it clean and the scratches off. Do you have any suggestions for my problem?
Ruth Sessions- Lake City, Florida
February 19, 2009
Hi, Ruth. I've never experienced any joy in trying to clean aluminum with any aluminum cleaner. If you have a grinder, or at least an electric drill, you can try putting a buffing pad in it and see if you can make any progress with a polish like Mother's Aluminum Polish [linked by editor to product info at Amazon]. Good luck.
Regards,
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |