finishing.com logo ips1
HOME FAQs BOOKS JOBS: Help Wanted Suggestions      you are here: Hotline/Forum => Letter 10001

Info about Spray Phosphating Systems

   

 

We have Powder coating plants. Also we use metal pretreating line for this (rust removing). But the current method is not very efficient for us, because it is dipping method. Therefore we want to know about spray method.

INDIKA P [last name deleted for privacy by Editor]
TRADING - SRI LANKA


May 22, 2008

Hi, Indika. Yes, spray systems are usually considered more efficient because the mechanical energy of the spraying makes for faster processing and sometimes better consistency.

There are a number of manufacturers of such phosphatizing systems, and these days you can get all-plastic construction if you wish. They essentially consist of nozzles for spraying the solution, inside of tunnels which collect the overspray and direct it back to the reservoir for pumping through the nozzles once again.

Good books about phosphating are Samuel Spring's "Preparation of Metal for Painting" [link is to info about the book at Amazon] and "Phosphating of Metals" [link is to info about the book at Amazon] by Werner Rausch. Good luck!

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search