HOME FAQs BOOKS JOBS: Help Wanted Suggestions you are here: Hotline/Forum => Letter 196
Electroplating for a school science project
----
My 5-year-old son wants to do a science fair project on plating. He saw someone on TV plating something and he asked me if I knew how to do it. When I was a kid, a science fair exhibitor plated copper pennies with silver. Do you know someone who can tell me how to do that? It seemed like a simple thing, but I don't know any details.
Darrell Ostler|
----
For this age group, Darrell, a simple immersion deposit might be more practical than electroplating. Get copper sulfate [linked by editor to product info at Amazon]. Then get some simple coins or small parts, clean them with toothpaste and a toothbrush (good to remind the kiddies anyway), then vinegar or lemon juice, rinse them well, and put them into the copper sulfate. Copper will deposit on them.
|
Naked Eggs & Flying Potatoes: |
|
S |
----
Thanks for posting my inquiry and the response. I think I will try the immersion method on a few nickels just to turn some heads. I would still like to do the simple electroplating on copper pennies though. My son gets very excited about electricity and batteries and such. In his mind, if a science experiment doesn't use electricity, it isn't science. So, do you have a simple "recipe" for silver plating some copper pennies? I know you are probably busy and would prefer to receive revenue generating inquiries, but I've looked everywhere and can't seem to find anyone who knows. The local plating shops don't want to give me the time of day, and you're obviously an authority. You are the best contact I've found. Anything you can do would be sincerely appreciated. Lastly, I think you have a solid web page. Not too flashy (which is good in my book), but it is packed with a lot of very useful information. Darrell Ostler--- My middle-school son wants to do a plating demo as a science fair project. And, yes, I did suggest this based on a demo I saw years ago. what I saw was plating of pennies using a silver spoon as an anode. We were led to believe the bath was simply water, although I now have come to learn that was just a bunch of hooey. I have followed your FAQ to the point of tracking down some (a couple of tablespoons full) silver nitrate, which, as it turns out, was no simple task! I've been to the library but the only bath I could find for silver plating didn't specify silver nitrate. Can you provide me with a formula for a small batch (1-2 liters) of solution? Is there anything else I need to add besides the silver nitrate and distilled water, and does the bath need to be heated or is room temperature enough? Lastly, do I need to use a silver source such as an old spoon or coin for an anode, or do I use a copper anode? Your site has been most helpful, and I really appreciate your response. Thanks! Dan Shogren--- Real silver plating is done out of cyanide, Dan, which is a horrible poison and out of the question for a home or school experiment. With silver nitrate you may form a poor deposit -- sorry, but I really don't know. But the Electroplating Engineering Handbook says that to prepare a standard silver nitrate test solution, dissolve approximately 17 g of silver nitrate in a liter of chloride-free water, and store in an amber bottle. While that test solution is not really meant to be used as a plating solution, it sounds like as good a formula as any :-) Silver may not be easily plateable from silver nitrate, but please let us know what you find. Good luck!
|
|
C |
----
Hello ... I have done a child's plating job with electricity by using dilute cobalt chloride solution from a kid's chemistry set. You can use either a piece of cobalt as the anode (usually not available readily), or a graphite rod out of an old d-cell battery. A 1-1/2 volt battery should do. Agitate the penny while plating. It will at least look vaguely silver to gray. Vince Summers |
|
I |
--
Folks, I suppose I'm just a kid at heart, but I'm one of those irresponsible science showmen who plate silver on things as a demonstration. My favorite is electroless silver plating on glass. It makes a great silver cup from a cheap glass and you can get a kit containing methyl glucamine through LON Lab, or you can use the older formaldehyde method with silver nitrate. For electrolytic plating, how about showing off the classic woods strike. The recipe is: 1 oz muriatic acid [linked by editor to product info at Amazon], 8 oz of water, and 1 oz of Nickel Chloride (often included in chemistry sets). Plate with 3 volts (two 1.5 V dry cells). You can tell the kids that this strike is extensively used in industry. Good Luck, Robert Buxbaum |
|
I |
--
I'm doing a science project, for my 4th grade class, on copper plating and I don't quite understand it, could you please help me? The experiment book I used says to take a small glass of vinegar and sprinkle in a few good shakes of salt. Then put in some dirty pennies. The pennies are cleaned of the surface corrosion. Then take a iron nail and clean it with steel wool [linked by editor to product info at Rockler]. Then put it into the glass. After 5 or 10 minutes the nail will be covered with a bright coat of copper. Can you help me explain what is going on? Thanks a lot for your help! Danielle [last name deleted for privacy by Editor]New Life Academy ---
I tried your experiment, but my pennies were not very corroded, so I may not have had enough copper in the water to see anything happen on the surface of the nail. This kind of reaction is very useful, and is used every day in science and industry to help make the things we use, making our lives easier and more interesting. The things that are happening in your little glass are much more complicated than this, so you must study very hard.
|
|
|
N |
(1997)
Here is what the Rochester branch of the AESF had been using for years as a plating demo at our annual Engineering Fair: bright nickel plating of pennies. Sure, the setup is not as basic as with copper plating, but no cyanide is required and the plate is bright. Watts-based bright nickel baths are pretty common in any local bumper plating shop (see your phone directory under "Electroplating services"). Pour some bright Nickel solution in a 1 l beaker, put it on a hot plate, get a small battery or rectifier and, in combination with the toothpaste and toothbrush cleaning technique described above by Ted - you are in business. Don't forget to rinse the pennies well before and after plating and return the plating solution back to the shop after you are done. Happy electroplating from PlaterB! ![]()
---- |
|
Z |
--
I am a high school chemistry student who is planning on doing a simple electroplating procedure for the class. I plan on plating zinc onto pennies. This seems to me to be much simpler than using silver. Am I correct in this assumption? Graham W [last name deleted for privacy by Editor]-- I would say yes because I can plate a fairly bright and adherent zinc coating from dilute acetate or sulfate solutions, and I don't know how to do this with silver. In reading the many letters on this subject, I am starting to believe that any demonstration of electroplating should include a demonstration of wastewater treatment. A nice graphite sponge cathode for electrolytic recovery would be neat. What good does it do to show someone how to plate, if we don't show the audience that plating requires a carefully thought out and implemented plan for wastewater treatment? Also mention that some plating processes, like chromium plating, for instance, also create a mist hazard for the operator, and this process requires ventilation and scrubbing of the air before release to the environment. What kind of references do you have in your high school for electroplating? Tom Pullizzi Falls Township, Pennsylvania -- I'm not sure what you mean by references; I have the Metal Finishing Guidebook and Directory. What is another metal that would be good to plate onto copper? Graham W [last name deleted for privacy by Editor]-- That is a very good reference, I did not expect you to say that you have one of those! There are many formulas in that book, but I don't know how many you can use in the home, since it is a reference for industrial users. So you have a powerful reference, now you need to control its power and design a good demonstration for high school level chemistry. Have you tried to plate anything so far? What were the results? Have you read the chapters on rinsing by our very own Ted Mooney, P.E., and on wastewater treatment? Tom Pullizzi Falls Township, Pennsylvania -- I'm glad to hear that you think so highly of it. I got it when I interviewed the president of a plating company. I have never even attempted to plate anything yet. I have read the chapter on rinsing, though I admit it got a bit too technical for me, though I'm sure if I had any experience rinsing it would probably make more sense. Graham W [last name deleted for privacy by Editor]-- Idea. Why don't you switch gears, and make your project about... RINSING! The world does not know enough about rinsing. Use your sources from electroplating to expand and expound on the subject of rinsing. Rinsing the soap out of laundry, washing the ice cream out of Breyers' containers. Show your fellow students how much it costs the earth to have clean cars and jeans. Hot water rinses much better than cold water for most projects, talk about the energy cost of rinsing and how it relates to global warming. It is a revolting subject, this rinsing, because the waste is a very dilute stream of milk, suds, metal ions, petroleum hydrocarbons, etc., but I volunteer you to solve some of our (all too human) problems. I will help as much as I can. Good Luck. - t p.s. You have plenty of experience in rinsing, now you have to look at the process as a scientist, and understand how it works. Something to do about that law on entropy. If you line up the atoms on one object, you have to disrupt the order of at least that many atoms somewhere else in the universe. Result: pollution. Tom Pullizzi Falls Township, Pennsylvania |
|
C |
--
I also have been trying to help my teenager with a science project. Many of the entries here have been helpful, but are scattered. I have some specific questions: 1.) Can one plate copper using a copper sulphate pentachloride solution? 2.) If so, at what strength, and at what temperature, and at what voltage. 3.) When using old developing solution to plate silver (silver nitrate): - do I need a silver anode? All my previous attempts have resulted in a dirty black target. note: My local camera shop reclaims their silver. It seems to be easy for them. Wallace Reid-- Yes, Wallace, the thread meanders. That's the nature of public participation, but we do have an FAQ on "How Electroplating Works" that is arranged in tutorial fashion and will be reasonably easy and straight forward to follow. 1. I think you meant copper sulphate pentahydrate, i.e., CuSO4.5H2O. Root Killer [linked by editor to product info at Amazon] is mostly comprised of 'copper sulphate pentahydrate'. This question was answered above, and it was a qualified 'yes' because we can't be 100 percent assured that a manufacturer might not decide to include something besides copper sulphate in the root killer (for example some organic biocide like a weed killer). 2. For the purpose of a school science project, use whatever strength you get, run it at room temperature for simplicity, and 1-1/2 to 3 volts. As long as it has a blue tint it should work fine. 3. I've never tried that one, but I do know that silver nitrate isn't used for real silver plating. I think the anode material is not critical, and see no reason to heat the solution or apply more than 1-1/2 to 3 volts. But there is a big difference between removing the silver from waste like the photo shop is doing, and producing a good silver plate. Good luck.
|
--
Would anyone please help me?
I'm desperately trying to find out how to electroplate a non-conductor, to be exact, a leaf. the leaf needs to be made a conductor so that a coat of metal can be deposited. does anyone know how to make the leaf a conductor? It needs to be placed in some kind of solution, but what?
I'd like anyone that can help. Thanks
Susanne de vaalthe Hague, Netherlands
|
--
Hello Susanne, We have an FAQ on how to plate organic materials. Lacquer the leaf so it will not be destroyed by the plating chemicals; spray on a "two-part silvering solution" where one component is a soluble silver compound and the other is a reducing solution; then start electroplating. Now, had you asked me how to create a Renoir oil painting, my advice would have been to dip a brush into paint, spread it on the canvas, and feather it in such a fashion as to give strong realistic romantic forms and surreal lighting. But I can't sketch a horse well enough that you'd be able to tell whether it was a cow or a dog I was aiming for. The point being, mechanical directions are 1 percent of the issue; the reason we find artwork beautiful is that we intuitively recognize that it is not a simple matter of cookbook motions; but, rather, a great amount of experience and technique, and sometimes extraordinary talent. Good luck.
|
--
I am attempting to immersion plate a copper penny with granular zinc in a solution of boiling sodium hydroxide. I used a 0.1 mol solution. Was this the correct molarity? When I conducted the experiment, one side of the penny became dull grey and the other side didn't plate at all. Do you have any idea why this was?
Graham W [last name deleted for privacy by Editor]--
Graham,
I hope this is something you are doing under proper lab conditions, with supervision. Boiling sodium hydroxide is really dangerous stuff, even without the zinc dust. This may not be something you should be doing for/with your high school class. But I don't see any such formulas in the handbooks -- where did you get it? Why are you doing this, Graham? There's a huge difference between electroplating pennies with zinc--using safe household chemicals like room temperature vinegar, as Tom described--and trying to use boiling caustic and zinc dust!
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |
--
I have already performed the experiment once. It was in one of our high school lab books, but the molarity for the sodium hydroxide was not given. This is my problem. I assure you that I have been performing it under careful supervision. I have been wearing safety equipment, and the sodium hydroxide I'm using isn't strong enough to be a very strong caustic. The zinc is mossy zinc, not zinc dust.
The plate just has not been very satisfactory. It should have turned out silver and was instead a dull grey. I'm perplexed as to why this is, and the only thing I can figure out is that the molarity I used was wrong. Do you have any ideas at all?
Graham W [last name deleted for privacy by Editor]--
I don't see the formula, or a similar one, in the guidebooks, so I don't know. But I'm surprised that you were able to get an immersion zinc plating onto steel.
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |
--
I was wondering how I can go about Electroplating a diecast car? I've tried to find books on it with no luck. Can you help me? I would like to Electroplate them gold and chrome but need some help. Please let me know if you can help. Thank you.
Jeff GriffithJeff:
There is plenty of info on that subject in the books here; suspect you have been looking in general science project books, etc., rather than in industry books. But the real answer to your question is that you can contact plating shops and have the cars plated for you. Working with cyanide and hexavalent chromium is no kind of hobby :-)
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |
--
I know exactly how to plate a copper penny with not only silver but brass!
First you clean the penny really well and don't touch it. Then you take about a gram of zinc shavings and mix that with 20 ml of sodium hydroxide and boil it on low heat. Once it starts to boil, drop in the penny and leave it there for around 10 min. It will turn a silver color. Then carefully take it out when it is totally silver (Still don't touch it) and rinse it off and dry it out for a bit.Then comes the cool part. You pick up the penny with tweezers and gently heat it with a propane torch. Be careful not to heat it too much or it will warp the penny. It about 5 seconds the penny will turn a shiny gold color!
I did this in school today actually, and it worked great! I'm only in 8th grade too, so this would make a good class experiment.
Andy B [last name deleted for privacy by Editor]