Need automatic buffing equipment, or training in buffing
----
I have a client who does replating and restoring of antique metal items such as lamps, kettles, and fixtures. Mostly with copper and brass finishes. They have a real bottleneck in the buffing or polishing area as this takes along time to get good at and is done by hand on a wheel. We are looking for new technology to speed up this process or training materials to get new people up to speed quicker. Thanks for the help!
Mike W [last name deleted for privacy by Editor]- Industrial Specialistoutreach center, Waterloo, Iowa
Automatic buffing machines are large and expensive and I really doubt that they will prove applicable for an assortment of parts like this, Mike. You might contact ASM International to see if they have a buffing course. But buffing is difficult, and it is perhaps best taught in an apprenticeship format, rather than as a crash course. Maybe one of our retired readers could conduct some longterm hands-on training for your client? Good luck!
Regards,
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |
----