(Cycles thru suppliers)


Letter 137

Rectifiers and ripple

-----

I have installed a system in house to electroplate the Advertising Jewelry we have manufactured for 30 years. We cast rubber molds using a tin/Lead alloy and a zinc alloy to create lapel pins, keytags, medallions, belt buckles, etc.. We plate utilizing a non cyanide strike, acid copper, nickle, gold, and non cyanide brass solutions. The question has come up about the deleterious effect of ac ripple in plating this type of product. What percentage of ripple is acceptable. I have been told by one source that under 10% is a must and by another source that 46% is acceptable and will have no effect in plating my kind of product. We have rectifiers that meter out to both percentages. Our experience for the last 60 days has been positive, but if it can be better, I would like to know.

Ken Fefferman
- Harwood Heights, Illinois


Ripple is generally considered problematical for nickel plating due to the possibility of generating a passive surface (with consequent delamination and peeling). To my knowledge (and it's only my understanding) ripple isn't a big problem for the more noble metals like copper and gold. Brass, being an alloy, will deposit more copper at low voltage, and more zinc at higher voltage, so ripple could be at least a theoretical problem. A better way of looking at the question, though, might be to ask yourself whether you picked appropriate rectifiers: single phase vs. three phase; tap switch (or powerstat) vs. SCR; operating near their maximum output (good), or being way oversized (bad). If you selected well in concept, I seriously doubt that you need to add ripple chokes, even to the nickel rectifier; if you selected poorly, you selected poorly even if ripple is not a problem. Give us some more particulars about the rectifiers if you get a chance.


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


Electroplating Engineering Handbook, Lawrence Durney


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com