Electroplating with niobium

-----

Although there is reference in the literature to the plating of titanium and its alloys I have not found anything that suggests it would be possible to electroplate these metals with niobium. Is there any experience of electroplating with niobium?

Richard Curtis



-----

Niobium is not mentioned in Safranek's "The Properties of Electrodeposited Metals and Alloys", nor is it listed in Faust's list of electroplateable metals in ASM's Electroplating course, or in ASM's Volume 5: Surface Engineering, the Metal Finishing Guidebook, or Durney's "Electroplating Engineering Handbook". If I had to bet on a guess, I'd bet on it not being plateable--but hopefully one of our readers will enlighten us both.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


++++

Niobium plating, in case you still interested in, go to Russian hand book 1987, F.F.Ajogin,page 310.


Cair Shishani
aircraft maintenance - Abu Dhabi, United Arab Emirates


March 2, 2010

According to old russian books niobium/ or niobium nickel alloys can be plated from solvent based electrolytes (DMF). Hope it helps and good luck!

Goran Budija - Zagreb,Croatia

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search