Letter 091
How to plate onto
Titanium
-----
I NEED TECHNICAL INFORMATION ON ELECTROPLATING PURE GOLD AND
PALLADIUM ONTO PURE TITANIUM. I UNDERSTAND THAT YOU HAVE TO CLEAN
TITANIUM AND YOU HAVE TO PROTECT THE SURFACE FROM OXIDIZING AGAIN
BEFORE ELECTROPLATING. CAN ANY ONE HELP WITH A PROPOSED CLEANING
PROCESS AND PLATING CYCLES. THANK YOU
ROY CONIGLIONE
-----
Hi, Roy. ASM International's "Metals
Handbook--Volume 5: Surface
Engineering has an outstanding chapter on how to plate onto
titanium and other hard to plate metals.
In addition, one method I know of is to nickel plate and then heat
the object to diffuse the nickel into the titanium. Letters
278 and
26878 offer some details on that. Good
luck with it.
|
|

Ted Mooney, P.E.
finishing.com