Using nickel anodes for nickel plating

-----

I am using a bright nickel plating solution that contains nickel sulfate. Should I use nickel anodes with this, I am not plating large things and my tanks are 2 gallons. I am worried nickel anodes will load the solution up with nickel to where it does not work as well. Please help. Thanks Rob

Rob G. [last name deleted for privacy by Editor]

Nickel anodes it is, Rob. The nickel does not dissolve except electrolytically. Talk to anode suppliers and get the right stuff.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search