Where does Boric acid go when nickel plating

-----

So, what happens to all the Boron from the boric acid as it is depleted in plating baths such as sulfamate nickel and bright nickel? Greg.    

Greg Watkins



-----

Well, most boric acid in Nickel plating gets lost through dragout and ends up in the wastewater as...you guessed it... still boric acid. Trace amounts of Boron, though, where found in various Ni electrodeposits, so some of it gets into the metal.


"PlaterB" Berl Stein
NiCoForm, Inc.

Rochester, New York

../Shops/industrial/nicoform.shtml




ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search