Need ruthenium plating by any deposition method
|
-----
I would like to communicate with anyone who is involved with the coating of ruthenium, or other platinum-group metals, onto other substrates. Any technique can be used, such as thermal spraying, electroplating, electroless deposition, etcetera. Regards Wayne G [last name deleted for privacy by Editor]University of the Witwatersrand Also interested in methods involving Ruthenium electroplating. Thanks, David W [last name deleted for privacy by Editor]USN - Bangor, Washington |
++++
Hello, Wayne. "Electroless Plating" by Mallory & Hajdu has a chapter on electroless plating of Platinum Group Metals, including a couple of pages specifically on Ruthenium.
Also, see letters 15711, 49098, and49150 for additional discussions on Ruthenium. Good luck.
|