ELECTROPOLISHING BASICS




COULD SOMEONE PLEASE SUPPLY ME WITH INFO ON ELECTROPOLISHING EQUATIONS, HOW TO CALCULATE THE TIME IN THE BATH VS AMPS,VOLTAGE PLEASE PRETTY PLEASE.

CRAIG ANDERSON
- AUSTRALIA
2001



Hi, Craig. The best coverage is in the Electroplating Engineering Handbook [on AbeBooks or eBay or Amazon (adv.)] . Lacking that,the Metal Finishing Guidebook has a good chapter. In-depth training is available from Metal Coating Process Company. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2001


Thanks Ted it helped a bunch.

C. Anderson
- Australia
2001




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"