Gold Electrophoretic Lacquer is Blistering


July 11, 2014

Q. We do Electrophoretic lacquers on metals.The metal substrate is carbon steel. Electrophoretic lacquer coatings are: Copper,nickel,silver and (30 micron) gold on metal substrates. We have some blisters on surface of our products. What advise do you have for a such blisters?
What causes to happen blisters in general and how we can prevent them?

Best Regards

Ebrahim Bohloli
- Tehran-Iran


July 22, 2014

Q. We do Electrophoretic lacquers on metals. The metal substrate is carbon steel. Electrophoretic lacquer coatings are: Copper, nickel, silver and (30 micron) gold on metal substrates. We have some blisters on surface of our products. What advise do you have forsuch blisters?
What causes blisters to happen in general and how we can prevent them?

Ebrahim Bohloli [returning]
- Tehran,Iran



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"