Hard chrome plating of engine liners step by step



September 14, 2012

Q. Hi!

Dear Sir,

I need your advise regarding the process of hard chrome plating of engine liner. Actually, I have hard chrome set up already ,i'm accepting plating job like hydraulic shaft and more on shaft but i have never tried on engine liner.

I will be grateful if you can share your ideas on how to do it in a step by step procedure especially on a porous process and finishing of an engine liner.

Hope for your reply.

Thanks!

Norman

Norman Medalle
- Cebu City, Philippines




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"