Surface prep for three-layer PE Coating on Duplex SS
Q. What is precaution required during surface preparation (type of abrasive), and 3LPE coating for Duplex stainless pipes?
Thanks
Mohamed Gaber
Coating Engineer - Cairo, Egypt
June 26, 2012
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.