Dacromet high strength bolts in contact with green concrete




Q. Dear sir, I'm Saiprasad. I want to know whether Dacromet bolts can be used in a steel member where the steel member is in contact with green concrete. Is there any reaction will take place between green concrete and Dacromet bolts? And if we can use Dacromet bolts, what's the life of the bolt used?

Thank You

Saiprasad Kudale
Design Engineer - Pune, aharashtra, ndia
January 31, 2012



March 12, 2012

Dear Mr Kudale,

What is green concrete? Do you mean Green Steel? Please elaborate.

Khozem Vahaanwala
Khozem Vahaanwala
Saify Ind
supporting advertiser
Bengaluru, Karnataka, India
saify logo



Hello,

ZInc aluminum flake coating with organic sealer top coat may help to protect the bolts for longer period.
You can try it.

kalyan dhakane
Kalyan Dhakane
Mumbai, India
April 6, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"