Electropolishing aluminium without perchloric acid
Instead of using perchloric acid and ethanol for electropolishing aluminium, what other chemical is suitable for electropolishing aluminium?
Noor Farah
Student - Malaysia
October 31, 2011
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.