Silver plating equipment for deep cavities and tubular parts




Hi to all. Could you recommend for me equipment capable of plating deep cavity parts and cylindrical parts, with a very good consistency in all the way of the part surface?
the size of the aluminum parts are 13" X 13", 6"deep.

Frank Martinez
buyer - California
August 18, 2011



Hi, Frank.

Electricity follows the path of least resistance, and the amount of plating deposited in an area is basically proportional to the amount electricity flowing to that area. So, to electroplate inside a tube you are going to need to have an auxillary anode running through that tubing. What sort of plating equipment and experience do you currently have?

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
August 19, 2011




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"