mobile?
Metal finishing Q&As since 1989
-----
Will nickel plated phosphor bronze pass salt spray if laser etched?
January 25, 2011
We are using the material C5191-H Phosphor Bronze with a nickel plating that needs to survive a salt spray test. Will this survive a salt spray test after laser etching?
Steve McGarry
designer - Vancouver, Washington
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.