Anodizing to MilStd 595 colours, 34094, 33446




RFQ: We manufacture satellite communications components requiring a durable RoHS compliant finish. We have solved electrical and microwave issues with anodizing, but we would like to offer military colours, specifically MilStd 595 green 34096 and tan 33446. There is also a requirement for suppression of infra-red reflection from the finish. Does anyone know if this is possible, and if so, who does it, or can you advise our local plating shop on the requisite process and materials? Thank you in advance for your time, effort and consideration.

Mike Stevens
product design engineer - White Rock, BC, Canada
December 1, 2010




RFQ: Were you ever successful in finding a supplier of this color? We are looking for an idea of a successful dye for this color.

Ian Kirk
manufacturing - Arlington, Washington, USA
May 2, 2012


A. It is possible to anodize to the military colors of the FEDSTD 595 #'s inquired above. Our company has provided this process to many customers in the Defense and Commercial Industries over the years.

Brian Murphy
Syracuse, New York
May 24, 2012




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"