Can anodized wheels be chromed or powder coated?





I was told that I can't powder coat anodized wheels, but can I chrome them? If so, black chrome?

Rado Ray
Auto club - Chicago, Illinois
April 29, 2010



Powder coating is applied over anodizing quite often. As long as your wheels are properly cleaned and prepped, there is no reason why they couldn't be powder coated.

Marc Green
Marc Green
anodizer - Boise, Idaho
May 8, 2010



sidebar

Marc, where is your dog?

James Watts
- Navarre, Florida
May 10, 2010



Finally had to put him down 2 years ago, James. Was just about the hardest thing I've ever done. He was 16 years old, and it was his time to go.

Marc Green
Marc Green
anodizer - Boise, Idaho
May 12



May 18, 2010

Ray,

I think you've got these backwards.

Anodized aluminum has a porous surface of of Al2O3 and AlOOH, which does not conduct electricity. You won't be able to establish a current for which to chrome plate, but powder coating should be fine.

Robert H Kinner
- Toledo, Ohio, USA




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"