Choosing sheath material of heating element: mild steel or iron




Thank you all guys for the information.
My question is in a situation where either mild steel or iron heating elements with sheath could pass the electrical tests and have equal prices, which one of them should be chosen for a small electrical household appliance?

Hoora R
- Rasht, Iran
December 13, 2009



December 14, 2009

Hi, Hoora. Mild steel is a more modern and widely available material which offers more flexibility, malleability, strength, and freedom from brittleness.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"