Poor throwing power of trivlent chrome




we had done the purification of trivalent chrome (white chrome) to remove the metallic contaminants by adding a complexing agent. the 'metal sludges' was then remove by filtration.
After the purification, we resume production ut found very poor/no coverage of trivalent chrome over ickel layer. And we found out the filtration was not properly conducted as we still found the yellowish stain at the filter cartridge.
is it the poor coverage caused by the improper filtration, as there might be residues of purifying agent in the bath?
Anybody has similar experiences?

Eng Chong Lim
Engineer - Johor Bahru, Johor, Malaysia
September 24, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"