Ring marks on arhaus mosaic top table




July 17, 2009

Hi,

I just bought an arhaus mosaic table top for $600 from a friend. I find old water marks on it. It is visible only at an angle. I tried the iron method but it did not work as it is old (I guess!). I feel awful about the marks as I cannot ask my friend about this.Please help....

TJ

Lakshmi Thiruvadi
buyer - Cleveland, Ohio, USA



Hi, TJ. Arhaus says the table top mosaic is "Hand-finished with a protective sealer". So you might ask them for advise on repairing or redoing the sealer. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
July 20, 2009



September 7, 2009

Emery cloth to polish out, sure it will take awhile, but it will match the rest of the surface.
If not, super fine steel wool or toothpaste to polish out.
Bit rougher, but will take the marks out.

Marc Banks
Blacksmith - Boone, North Carolina




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"