Need system for Reel to Reel wire electropolishing of nickel alloys





July 14, 2009

We are producing Nickel alloy wires. Some of the applications like glass sealing require the wire to be mirror finish. I think EP can be a solution. We are also producing Nickel plated steel wire for lighting industry and have lot of experience in plating of wires but no experience of Electro polishing.
Can someone give me a lead for equipment supplier, process, chemicals etc for EP.
Our wire is in reels of about 50 kg and we need a machine which can EP from reel to reel. Wire dia is 0.4 to 1.0 mm and as I said before they are NIckel, Nickel Manganese, Nickel iron (50/50).

Kamal Baid
We are a wire plater - JAIPUR, India




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"