OABIC, OIA, and BRUT finishes in anodizing




March 30, 2009

Hi,
Thanks in advance for your time.
I would like to know what is OABIC, OAI, BRUT finishes in aluminum anodizing? How they are different from Type 1,2 & 3 of Aerospace specifications?

Do they imply any specific process or just color codes?

Biren Desai
plant manager - Bangalore, India




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"