Artist wants to use silver x-ray film




I am a visual artist experimenting with exposed and non exposed x-ray film. How can I tarnish, or bring out the silver qualities in the film?
Thank you.

Karen Feuer-Schwager
artist - Laguna Beach, California
February 18, 2009



I suggest that you google 'Posterisation' and 'Solarisation'. Then try 'Darkroom techniques'.

geoff smith
Geoff Smith
Hampshire, England
March 3, 2009




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"