Nickel anodes for Nickel free plating?




As we are in the jewelry industries some European country's request for nickel free plating, We got down nickel free plating chemical from a reputed establishment.The inquiry is they told us to use nickel anode that really worries us because its back again nickel in the bath.Please educate me on this.

Mohamed Nuwais
Employee - Sri Lanka
March 3, 2008


Your concern is totally valid. You should not use nickel anodes. Perhaps neither their solution until you know exactly what they sold to you. G. Marrufo-Mexico

Guillermo Marrufo
Monterrey, NL, Mexico
March 5, 2008



Hi There,

Check with the supplier whether they gave you white bronze, or Palladium bath, there is no question of using Nickel Anode, it has to be Graphite or Carbon insoluble anodes.
Regards,

praveen kumar
Praveen Kumar
plating process supplier
Mumbai, India

March 7, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"