Is rhodium magnetic?




Is rhodium magnetic? if you get enough rhodium plating on gold to turn it white gold it will be picked up by a magnet.for which this is not silver.so if magnet picks up gold is because there is a lot of rhodium on it.now I wonder to first question .is there nickel in the rhodium liquid?or is rhodium magnetic?

curious

Marty Dolobach
pawnshop - Port Richey, Florida, USA
February 9, 2008



Rhodium is not magnetic, Marty, and there is no nickel metal in rhodium plating solutions. However, it is not unusual to electroplate nickel onto the object before plating rhodium onto it, and nickel is magnetic.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
February 22, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"