Having problem plating on polyester




January 12, 2008

Hi , I am Seyyed Mohammad Jahed, and I have experience plating on metals.my job is to make arts and statues.I use silver as the material, but I recently decided to use polyester.
But I don't know how to plate polyester because its not conductive.
I am free to any suggestion.
thanks

Seyyed Mohammad Jahed
arts and jewellery manufacturer - Sharjah, UAE



Please see our FAQ on plating organic materials. It introduces the various technologies that are used and may enpower you to go on to choosing a technology and then posing more specific questions. Good luck.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
January 22, 2008




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"