Best Wrap to Preserve Clean Shiny Silver





2007

We have just spent many several hours cleaning our sterling silver service using the aluminum, soda, salt mixture that was recommended on this site (letter 14502).

What is the best and most economical way to preserve the shine on the sterling silver after it has been cleaned? What can we wrap it in that will not damage the silver?

Thanks for your help.

Papamel

Meldrum J. Harvey
Consumer - Owensboro, Kentucky, USA



First of two simultaneous responses --

Pacific silvercloth.

jeffrey holmes
Jeffrey Holmes, CEF
Spartanburg, South Carolina
2007



Second of two simultaneous responses --

Try 3M siver protector strips-one of authorized USA distributors is Marsha Whitney Care Products,St.Paul, MN. Hope it helps and good luck!

Goran Budija
- Cerovski vrh Croatia
2007


Pacific Silvercloth is very good product,too. Hope it helps and good luck!

Goran Budija
- Cerovski vrh Croatia
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"