Protecting copper and brass from corrosion by epoxy resin and varnish in sea water [Saudi Arabia]





2007

Dear Sir

I am a doctora student of corrosion engineering in girs College of eduction in jeddah. I want books or courses in protiction copper and brass from corrosion by epoxy resin and varnish in sea water and soilin HCL,NaOH,NaCl

Thank you & Regards

Saidah Al-mhyawi
girs College of eduction - Jeddah, Saudi Arabia



2007

Hi Saidah,

Shell used to, maybe still have, an EPON 828 epoxy resin
which, they said, would bond to and cure under (sea)
water.

Maybe, I dinna ken, all the epoxies are like this ... this you'll have to ascertain.

Hope this helps.

freeman newton portrait
Freeman Newton [deceased]
(It is our sad duty to advise that Freeman passed away
April 21, 2012. R.I.P. old friend).





(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"