Homemade browning agent for antique brass/bronze



I have some new brass and bronze parts. I need to antique them to match original dull chocolate brown. any homemade solutions? also finished parts will be clear coated.

Ken Stephens
antique restoration - Saint Ignace, Michigan, USA
2007


Try www.thelitterbox.org website-there you can find 7 download free techno-chemical recipe handbooks(chapters on metal colouring),or www.archive.org/- old handbook on metal colouring by A.Hiorns,one old American handbook on same subject,or Langbeins handbook on electroplating(very good chapter on metal colouring)!Hope it helps and good luck!

Goran Budija
- Cerovski vrh Croatia
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"