mobile?
Metal finishing Q&As since 1989
-----
Uniform Hard Chrome Layer
We want to hard chrome plate a layer of 15-20 microns on a 35 mm dia shaft 30 inches long as uniform as possible. kindly suggest a suitable fixturing technique to do the same.
Thanks
VIKRAM
Vikram Dogra
Irusha India - Chandigarh, India
2000
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.