Metal finishing Q&As since 1989

-----

Removing clear topcoat while leaving underlying auto paint




have a 1991 Camaro that is in good condition other than the clear coat is wanting to come off --any suggestions on how to remove this without damaging paint ?

thanks

russell jones
hobbyist - high view, West Virginia usa
2007



The clear coat is coming off because the underlying base color coat is badly damaged by sunlight. The only fix is repaint.

jeffrey holmes
Jeffrey Holmes, CEF
Spartanburg, South Carolina
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"