Hello,
we are looking for a special sand-blasting material which is called : SCW Does anybody know about it?
Frank Kuepper
- Hilden, NRW, Germany
2000
SCW = Stainless Cut Wire
Available from Vulkan Industries (and others).
Adam Schrader
- Middle Haddam, Connecticut
January 11, 2010
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.