Stainless Steel Surface Finish How-To?



I want to impart a rough, random finish, by hand (no power tools), to 24 gauge stainless steel sheet. The area to be finished is about 24" x 36".

So far, 3M Scotchbrite #7440 is the roughest material I've found but it's still not enough.

Any suggestions on some alternate products and/or materials I can try next?

Randy Wayne
artist - Houston, Texas
2007



Sandblast?

jeffrey holmes
Jeffrey Holmes, CEF
Spartanburg, South Carolina
2007




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"