White streaks in bright dip
Can anyone tell me why we get white milky look after bright dip. the desmut will not take it off.
Race Ritchie
manufacturing - Odessa, Texas
2007
The bright dip solution is aged. The dissolved content is too high
John Hu
- Singapore
2007
![automatic anodizing banner]()
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.