2006
Hi,
I would like to coat a bearing cage with EN/PTFE to reduce friction between the cage and the bearing track.
What is the max working temp for EN/PTFE (its an engine core bearing)?.
Thanks.
Nir Ge
Engines - Tel Aviv
No appreciable changes up to 250 °C either in the Teflon or the nickel matrix. What kind of engine, by the way?
Guillermo Marrufo
Monterrey, NL, Mexico
2007
finishing.com is made possible by ...
this text gets replaced with bannerText
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.