Passivation Problem on Surgical Instruments




2006

Dear Sir,

We are the manufacturer of all kind of surgical instruments. Our instruments our customers are like very much that is why they are not leaving us. Our customers are importing the instruments from us but they passivation yourself they really like our instruments quality. But we want to passivation ourself. So, please help me and let me know what is the chemical for passivation and how we can be use?

Waiting your early reply,

Jamil Nawaz
- Pakistan



Nearly all of the surgical instrument companies in Germany are using citric acid based products that we sell to them. This is the state of the art. If you contact us I can give you the name of a distributor in Pakistan.
You can see ASTM A967 for details.

lee kremer
lee kremer sig
Lee Kremer
Stellar Solutions, Inc.
supporting advertiser
McHenry, Illinois
stellar solutions banner
2006


none
www.finishing.com is made possible by supporting advertisers ...
this text gets replaced with bannerText
spacer gets replaced with bannerImages



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"