Specification ZNIA3L-Silver for Coating?
2006
I want to know the specification of the following coating.
ZNIA3L-Silver
Whether the above specification is Zinc Flake Coating. If so equivalent
Dacromet or Geomet Coatings specifications.
V.V. Jambunathan
fasteners - Chennai, Tamil Nadu, India
adv.: Dip-spin Coating Services
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.