mobile?
Metal finishing Q&As since 1989
-----
Powder Over Autodeposition
2006
Has anyone had success powder coating over an autodeposited coating with good inter-coat adhesion?
I've tried a typical polyester powder and it didn't stick very well.
Thanks,
Robert Littlefield
- Clearfield, Utah , USA
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.