Deposition of tungsten.




Can anyone recommend a company that performs electrodeposition of tungsten?

James Intrater
- Fremont, California
2000


Tungsten would normally be deposited using sputtering from a solid target or chemical vapor deposition from WF6. I've never heard of anyone plating it in the pure form.

Jerry Zimmer
- Mountain View, California
2000




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"