Plating stainless steel with gold




2006

Please I want to make some stainless steel( forks and knifes ) gold plated
I have about 4200 pieces. I want the steps to make it gold plated
thank you

Fadi Taha
silver plated items - Beirut, Lebanon

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




Hello, Fadi. If you cannot locate a shop that can do this for you, start with the gold plating chapter of the Metal Finishing Guidebook, and also look up and read about cleaning cycles and Wood's Nickel Strike in the same book. With that general background under your belt, feel free to ask any specific questions you may have. Thanks.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"