mobile?
Metal finishing Q&As since 1989
-----
Selective etching of Ag (silver)
2006
Hi,
I am using Ag film as electrodes on Alumina membrane for electrodeposition. I want to know if there is a selective etchant for Ag which will not etch Ni or Pb present inside the pores of Alumina membrane
Thanks,
Nitesh Kumar
Pennsylvania State University - University Park, Pennsylvania, USA
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.