Specimen preparation for electrochem testing




2006

I have any confusion for specimen preparation for my research. I've read any standard for electrochemical testing but they don't describe any specimen preparation clearly. I wanna know complete standard that was established freely. And I'd like to know any site that published paper about electrochemical testing especially for steel.

Thank for your attention

Yours sincerely,

Beni Maolana
Metallurgy Laboratory ITB - Bandung, West Java, indonesia



Hello Beni. Just as there are 1001 different applications for steel, there are 1001 different tests to determine if the processes were satisfactorily performed for the intended application. Sorry, but I just don't know what you mean by "electrochemical testing especially for steel". What is it that you are trying to determine, and why?

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2006




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"